Heating Elements

CSM provides a wide range of tubular heating elements for industries as diverse as the food and beverage and chemical processing sectors. Our heating elements can be customised to suit the needs of individual clients, with thicknesses ranging from 0.3mm to 1.5mm (depending on diameter), and diameters varying from 4mm to as much as 28mm.

Heating elements can be manufactured in a variety of shapes, allowing clients to fulfil their unique heating requirements. They also come in a variety of alloys, including AISI and high nickel materials. So if clients require elements with low corrosion rates, CSM are in a position to meet their needs.

Additionally, we can supply heating elements made using heat-treated steel. We use an in-line induction oven functioning at 1050 degrees centigrade, which exceeds the recrystallisation temperature and provides reliable results. This allows us to satisfy clients who need elements with high strength and corrosion resistance.

Suitable products


  Thickness (inch)
Diameter (inch) 0,012 0,016 0,020 0,024 0,028 0,031 0,035 0,039 0,047 0,059
0,157              
0,197                    
0,236                    
0,250                    
0,275                    
0,283                    
0,295                    
0,315                    
0,335                    
0,354                    
0,375                     
0,394                    
0,413                    
0,433                    
0,453                    
0,465                    
0,472                    
0,500                    
0,512                    
0,524                    
0,543                    
0,551                    
0,571                    
0,583                    
0,591                    
0,610                    
0,625                    
0,630                    
0,669                     
0,685                     
0,709                     
0,750                     
0,787                     
0,827                    
0,839                    
0,866                    
0,875                    
0,906                    
0,945                    
0,984                    
1,000                    
1,059                    
1,102                     
Diameter (inch)  0,012 0,016 0,020 0,024 0,028 0,031 0,035 0,039 0,047 0,059
  Thickness (inch)
    Chemical Composition
    C\% <= Si \% <= Mn \% <= P \% max S \% max Cr \% min - max Ni min - max Others
AISI 304 EN 1.4301 0,07 1,00 2,00 0,045 0,015 17-19,5 8-10,5  
AISI 304L EN 1.4307 0,03 1,00 2,00 0,045 0,015 17,5-19,5 8-10  
AISI 321 EN 1.4541 0,08 1,00 2,00 0,045 0,030 17-19 9-12 Ti min.= 5 x \%C
AISI 316L EN 1.4404 0,03 1,00 2,00 0,045 0,030 16-18,5 10-13 Mo = 2-2,5
AISI 444 EN 1.4521 0,02 0,4 0,4     17,7   Mo = 21
Ti+Nb = 0,45
AISI 316SL EN 1.4435 0,03 1,00 2,00 0,045 0,030 17-19 12,5-15 Mo = 2,5-3
AISI 316Ti EN 1.4571 0,08 1,00 2,00 0,045 0,030 16,5-18,5 10,5-13,5 Mo = 2-2,5
Ti min = 5x\%C 
AISI 310S EN 1.4845 0,08 1,50 2,00 0,045 0,030 24-26 19-22  
AISI 309 EN 1.4828 0,04 1,50÷2,50 2,00 0,045 0,030 19-21 11-13  
Alloy 800 EN 1.4876 0,04÷0,08 0,02÷0,06 0,50÷1,00 0,015 0,010 19-21,5 30-32 Al\% = 0,2-0,4
Ti\% = 0,2-0,5
Alloy 840 EN 1.4847 0,05 1,00 1,00 0,015 0,005 19-22 19-22 Al\% = 0,6 max
Ti\% = 0,6 max
Alloy 825 EN 2.4858 0,025 0,50 1,00 0,020 0,010 19,5-23,5 38-46 Al\% = 0,2 max
Ti\% = 0,6-1,2 max
Alloy 600 EN 2.4816 0,05÷0,08 0,50 1,00 0,015 0,015 14-17 min 72 Al\% = 0,3 max
Ti\% = 0,3 max
Alloy 601 EN 2.4851 0,03÷0,08 0,50 0,80 0,020 0,01 22-24 58-63 Al\% = 1,1÷1,6
Ti\% = 0,1÷0,4

We are able to provide HEAT TREATED tube, the treatment is made with an "in line" induction hoven working at 1050°C, working in a protect atmophere above the re-crystallization temperature.

 